S275?suitable for numerous general engineering and structural applications
S275 & S275JR steel can be supplied in plate, round bar and flat bar. S275 provides a lower strength (than S355) but has good machinability and can be welded. The average minimum yield for S275 steel is 275 N/mm? giving its name: S275.
BS EN 10025 S355, S355JR, S355J2 and S355J2 N supercedes BS4360 50A, 50B, 50C 50D